NMR Tubes, 10 mm, Wilmad, Precision | Thin-walled Precision NMR Tubes. To maximize Signal-Noise-Ratio, Precision NMR Tubes have minimal paramagnetic impurities that would impact shimming. For experiments requiring critical shimming quality (high/ultrahigh field, nonspinning, multi-dimensional, multi-nuclei, DNP experiments and studies involving biological samples). - Made from borosilicate glass, ASTM E438, Type 1, Class A
- Hydrolytic class 1
- Inner surface is resistant to strong acid and base at ambient temperature
- For temperatures up to 230 °C and within a temperature step of 120 °C
- Include disposable caps
|
|
|
Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 8.90 mm ± 0.13 |
---|
Length mm | 178 |
---|
Wall thickness mm | 0,55 |
---|
Frequency | 100 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 178 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 200 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 203 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 200 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 178 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 300 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 178 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 400 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 203 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 400 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 229 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 400 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 178 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 500 MHz |
---|
| | | Ext. Ø | 9,9935 mm ± 0.0065 |
---|
Int. Ø | 9.070 mm ± 0.013 |
---|
Length mm | 203 |
---|
Wall thickness mm | 0,46 |
---|
Frequency | 500 MHz |
---|
| | |
|